Typical Nitriding Materials

The typical materials we recieve for Nitriding are:
-4140, 4150, 4340, N135 – Nitralloy – Alloy Steels
-H-11, H-13, D-2, S-7, – Tool Steels
-303, 304, 347, 410, 420, 440, 501, 15-5, 17-4 – Stainless Steels
We also do Malcomizing and Vascomax 300
Our typical turn around time for H-11 or H-13 materials is within 24 hours, with the result of a case depth ranging from .005 to .007 and with a surface hardness of 15N 93,94.
Surface Treating of Ohio has processed parts for the Automotive, Construction and Mining industires, please feel free to Contact Us to see if there is something that we can do for you.